Share
Stress Corrosion Cracking Behavior of EV31A and Mg-Mn Magnesium Alloys
Padekar Bharat (Author)
·
LAP Lambert Academic Publishing
· Paperback
Stress Corrosion Cracking Behavior of EV31A and Mg-Mn Magnesium Alloys - Padekar Bharat
$ 69.94
$ 83.05
You save: $ 13.11
Choose the list to add your product or create one New List
✓ Product added successfully to the Wishlist.
Go to My WishlistsIt will be shipped from our warehouse between
Friday, July 05 and
Monday, July 08.
You will receive it anywhere in United States between 1 and 3 business days after shipment.
- 0% (0)
- 0% (0)
- 0% (0)
- 0% (0)
- 0% (0)
All books in our catalog are Original.
The binding of this edition is Paperback.
✓ Producto agregado correctamente al carro, Ir a Pagar.